Cavity wall ties: what they are and how they work
Every cavity-walled house in the UK is held together by small metal ties you never see. This guide explains what they do, which ones are in your walls, and what happens when they fail.
A cavity wall tie is a metal connector bedded into the mortar joints of a cavity wall. It spans the gap between the outer leaf (usually brick) and the inner leaf (brick or block), so the two thin walls act as one and share the load from wind.
How a cavity wall works
A cavity wall is two separate skins of masonry with a gap between them. In older houses the gap is usually 50 to 75mm. Rain that soaks through the outer leaf runs down the inside of it and out at the bottom, so it never reaches the inner leaf and your rooms.
Cavity walls became common in UK housebuilding from the 1920s and were the norm for new houses by the middle of the century. Many now have insulation in the cavity as well.
Buying a house and the survey has mentioned wall ties? See what to do when a survey flags wall ties. Buying ties for a new wall? See choosing ties for new work.
What the ties do
Each leaf on its own is only one brick or block thick, which is too slender to stand up to strong wind. The ties lock the two leaves together so that wind pushing or sucking on the outer leaf is shared with the inner one, which is also held by the floors and roof.
- Restraint: they stop the outer leaf leaning out or falling away.
- Load sharing: they let both leaves resist wind together.
- Keeping the cavity clear: the drip in the middle of a tie sheds water, so it does not bridge damp across the gap.
How many ties a wall has
Ties are laid into the bed joints (the horizontal mortar joints) as the wall goes up. For a cavity wall in brick or block, the usual pattern under Approved Document A of the Building Regulations is one tie every 900mm along and every 450mm up, staggered. That is about two and a half ties for every square metre of wall.
Extra ties go beside window and door openings, movement joints and roof verges. Wider cavities take longer ties, not closer spacing. The full detail is on the wall tie types and spacing page.
How long they last
Modern ties are stainless steel and are made to last the life of the building. The problem is the ties in older houses. These were usually mild steel with a zinc (galvanised) coating, and once the zinc has gone, the steel rusts.
Research by the Building Research Establishment (BRE), published in 1981, found that ties galvanised to the minimum then required were likely to corrode sooner than had been assumed, and the required zinc coating was increased that year. That is why wall tie failure is a known risk in cavity-walled houses built before then.
The rest of this guide
Standards and sources
- Approved Document A (Structure), the government guidance on meeting the structural parts of the Building Regulations in England, including wall tie spacing.
- BS EN 845-1, the British and European standard for wall ties and other masonry ancillary components.
- BRE Digest 401, Replacing wall ties, and BRE Digest 329, Installing wall ties in existing construction, the Building Research Establishment's guidance on diagnosis and remedial work.
- Wall Tie Installers Federation (WTIF), the UK trade body for remedial wall tie installers, founded in 1989.
Questions people ask
What is a cavity wall tie?
A metal connector bedded into the mortar joints of a cavity wall. It spans the gap between the outer and inner leaves so the two leaves work together and resist wind.
How long do wall ties last?
Modern stainless steel ties are made to last the life of the building. Older galvanised steel ties, especially those from before 1981, often corrode well within it. See wall tie failure.
Does my house have wall ties?
If it has cavity walls, yes. Most UK houses built from the 1920s onwards have cavity walls. Solid walls, usually about 225mm thick with brick ends (headers) showing in the pattern, have no cavity and no ties.
Are wall ties a structural problem?
Failed ties are. Without them the outer leaf of brickwork is no longer restrained, and over time it can crack, bulge and in severe cases fall, especially in high winds.